BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • ADJUSTABLE STOOLADJUSTABLE STOOL
    Equally uncomfortable to sit and when feet do not reach the floor and if the seat is very low. I think everyone has noticed that, sitting behind the piano, the pianist is rotating the...
  • PLANE FOR TWOPLANE FOR TWO
    Since the days when "Tsar Peter arapa married", carpentry work associated with a large number of planing boards or timber, produced a two-handed plane. Such a tool would no doubt be...