BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • AIRFRAME F1-AAIRFRAME F1-A
    Among the priority directions of search to achieve the best results in athletes performing in class gliders F1-A, now in a special place is dinamalar — because of its effectiveness and...
  • THE TILES RESCUED… IRONTHE TILES RESCUED… IRON
    Happened that my electric "Rossiyanka-2" went out on one of the switches controls the degree of heating burners. So much so that no restoration is not subject. A suitable replacement for...