BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • “MOUSE” FOR TWO“MOUSE” FOR TWO
    The first little micro-car "mouse" I built for my kids. As a result, I accumulated some experience of designing and has already planned not as a child, and "adult" car. Called it...
  • EVEN SILK, THOUGH THE SKINEVEN SILK, THOUGH THE SKIN
      For sewing normal sewing machine materials such as tough leather or canvas, offer to complete the regular presser foot or to make a new one. It is necessary that the cloth was not...