BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • TO DRY TO SMOKE? PLEASE!TO DRY TO SMOKE? PLEASE!
    To dry mushrooms, fruit, or smoke, for example, meat, fish — not from an ambulance. And troublesome, tiresome to make sure that the process went properly and the result was good food for...
  • LATEST CRUISER TANKSLATEST CRUISER TANKS
    In the period from 1937 to 1945 in service with the British army consisted of only four types of infantry tanks. Changing models of military vehicles cruising type resembled a...