BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • THE SHEARERS, NOT ONLYTHE SHEARERS, NOT ONLY
    Shearing machines МСУ200 with a built-in handle three-phase asynchronous motor (200 Hz, 36 V, 100 W, 12, OOO rpm) we have in the village is not uncommon. Though slightly modified,...
  • With forced airWith forced air
    With the help of articles in the magazine «Modelist-Konstruktor», I built myself a universal power tiller based on a Minsk motorcycle. It turned out to be a good, hard-working mechanical...