BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • TABLE – MATRYOSHKATABLE – MATRYOSHKA
    Even in small apartments on special occasions are big companies, and then there is the problem of the table — are available, bring from neighbors. The proposed table for the living room...
  • QUITE INDEPENDENT “TODDLER”QUITE INDEPENDENT “TODDLER”
    Talking about the rapid development of cruiser forces such Maritime giants like Britain, Germany, France, Russia, it would be unfair to forget about a much more modest powers of Europe,...