BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • THE ROCKET PLANE “THE DUCK”THE ROCKET PLANE “THE DUCK”
    According to the rules of the competition model rocket must use only during takeoff the thrust of a jet engine, and the descent of the lifting force of the aerodynamic surface. For...
  • “COMPACT -800” MOTOR FOR ALS“COMPACT -800” MOTOR FOR ALS
    Numerous rallies of Amateur aircraft collected hundreds of enthusiasts, small aircraft, and it clearly showed that the interest in the design of Amateur aircraft huge. However, in...