BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • Cottage TravelerCottage Traveler
    M-K has repeatedly published descriptions of car trailers. And industry produces them, for example, “Skif”. However, I decided to build it to my own taste. And since then, the traveling...
  • “COAT” FOR DOOR“COAT” FOR DOOR
    I want to offer the readers I used in the method of the door trim: it is simple, inexpensive, convenient and allows you to achieve a good zvono and heat insulation front door. And...