BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • “FIFTEEN PUZZLE” ON THE WATER“FIFTEEN PUZZLE” ON THE WATER
    Water motorcycles, or scooters, are very popular among water motor sports enthusiasts and athletes. This type of transport has expanded the range of watercraft, contributes to the...
  • FLOUR GRINDER…FLOUR GRINDER…
    Increasingly, the editor receives letters and phone calls with the same request — to publish drawings and to talk about how to make your own hands a simple mill. The need for this device...