BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • FLOWERBED IN VARIATIONSFLOWERBED IN VARIATIONS
    Flower garden in front of the house or plot is usually round, oval or rectangular bed edged diagonally dug brick. It forms a jagged fence, holding an earth mound from fraying....
  • TO HIT WITHOUT DAMAGINGTO HIT WITHOUT DAMAGING
    If you want to align a dent in the soft metal or use a hammer in a similar situation where he can hurt the surface of the material, — wear it "soften" a shirt of leather or thick rubber:...