BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • MINI PLANERMINI PLANER
    For processing small crafts of wood and plywood a very handy tool may be Rubanchik, which is easy to make yourself.   The housing 1 (see Fig.) cut out of copper or bronze with a...
  • LAMP-PETALLAMP-PETAL
    Original table lamp can be made in one evening, and it will require only a small sheet of thin iron. He will perform the role of the base, and a lampshade, and a reflector. Enough at...