BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • POUR TRANSISTORPOUR TRANSISTOR
    The heat of summer. The sky is cloudless. Without irrigation the garden can not be saved. In this case, it is good to use a plant that waters itself. The device is an electronic relay on...
  • ZIS-101ZIS-101
    The name of the Plant named after Stalin (the former AMO), which produces trucks and buses, has received in 1931. The first attempt to organize the production of passenger cars took...