BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • A WOODEN SOLEA WOODEN SOLE
    no Doubt — metal tool for flat planing of wood — all sorts of planers, jointer, etc. — has its advantages: does not warp from moisture easy to work with, reliable. However, even if it is...
  • TABLE HEADSETSTABLE HEADSETS
    These simple wooden design for dining table complements the meal not only in the countryside but in a city apartment — so nice they look, not to mention their functional need. Really,...