BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • ELECTRONIC IGNITION:OPTIONSELECTRONIC IGNITION:OPTIONS
    We are talking about different versions of electronic ignition devices (UEZ), is made as transistors and IC. The lack of scarce elements, as well as the simplicity of the schemes allow...
  • “RUNNING LIGHTS”“RUNNING LIGHTS”
    A variety of light device (sdes), from the simplest to the most complex — widely used for the decoration of Christmas trees, holiday youth parties and even school discos. Therefore, the...