BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • Play structures in the yardPlay structures in the yard
    How can you equip a children's playground in the yard? You can simply install a sandbox, a slide, or carve figures of fairy-tale and cartoon characters from logs. But that is not the best...
  • GAZ-21 “Volga”GAZ-21 “Volga”
    At full capacity, the Assembly line of the Gorky automobile plant, producing the new cars GAZ-21 "Volga", earned at the end of April 1957, although the first three machines of this type...