BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • THE SECRET PROFESSION OF “DIPLOMATS”THE SECRET PROFESSION OF “DIPLOMATS”
    "Three potatoes, two beets, a kilo of carrots, two heads of cabbage"—a tongue Twister rattled off the seller standing in front of me a slender youth. I looked doubtfully at him, mentally...
  • WITCHEDWITCHED
    Skis kept slipping off... Leaning on a stick, he made a hesitant step forward, but only tried to pull foot slipped, and I had to start all over again. I waved to him, and, intending to...