BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • New Generation GliderNew Generation Glider
    This small aircraft attracted attention at the Tushino International Salon in June 1995. It differed from other similar ones in its somewhat unusual layout. In a conversation with its...
  • SeAZ-11116SeAZ-11116
    The car VAZ-1111 "Oka" was put into production in 1988 — assembling the machine was carried out at the Kama and the Volga factories. Further production of the car and joined the...