BRAZED ALUMINIUM

BRAZED ALUMINUMModernizing the conventional electric soldering iron, can safely be taken for soldering aluminum products, And the quality of the weld and the process practically does not differ from traditional. Finalizing undergoes only the copper core of the soldering iron. His working part should be dulled with a file before the formation of the pad width of about 4 mm, in which a saw make a longitudinal propyl depth of 7-8 mm. Of the saw blade, tempered in the fire, cut a section length of 12 mm and treated with a mixture of 20% sulfuric and hydrochloric acids to remove surface scale. Then cut the fabric insert propyl soldering iron and fix in a Vice. Made the tip serves as a scraper for removal of oxide film with zalivaem the surface of aluminum.
 
A. VICTOR, N. MELAMUD, Odessa, Ukraine

Recommend to read

  • BRO-11M – A STEP TO THE SKYBRO-11M – A STEP TO THE SKY
    Did you know that many amateur-built aircraft have the BRO-11M glider as their basis - the initial training glider from the well-known Lithuanian aircraft designer B.I. Oshkinis? Quite...
  • TRIANGULAR STOOLTRIANGULAR STOOL
    In the apartments of mass developments of the past years of food is very petite in every square decimeter. In these areas put only the furniture, without which one cannot do. And if the...